河南龙翔标志Henan Longxiang Petroleum Additives Co., Ltd.Oilfield Chemical Additives

Product Details

油井用水泥Filtration-Control Additive

A filtration-control or fluid-loss additive designed to improve mud-cake quality and reduce fluid invasion.

Function
Fluid-Loss Additives

Actual specifications are subject to supply confirmation.

油井用水泥Filtration-Control Additive

Performance Information

Swipe horizontally to view the full table.

表 1 油井水泥降失水剂理化性能要求
项 目指标
固体液体
外观流动粉末均一液体
水分,% ≤8.0—
固含量,% ≥10.0
细度(筛孔 0.315mm 筛余),% ≤12.0—

Swipe horizontally to view the full table.

表 2 加有中温型降失水剂的水泥浆和水泥石性能要求
项目指标
一级品二级品
失水量,mL ≤50.0150.0
初始稠度(80℃、46.5MPa 、45min),Bc ≤30
40~100Bc 的时间,min ≤30
游离液,% ≤1.4
抗压强度(102℃、20.7MPa 、24h),MPa ≥14.0

Swipe horizontally to view the full table.

表 3 加有高温型降失水剂的水泥浆和水泥石性能要求
项目指标
一级品二级品
失水量,mL ≤50.0150.0
初始稠度(120℃、73.9MPa 、61min),Bc ≤30
40~100Bc 的时间,min ≤30
抗压强度(144℃、20.7MPa 、24h),MPa ≥14.0

Swipe horizontally to view the full table.

表 4 加有超高温型降失水剂的水泥浆和水泥石性能要求
项目指标
失水量,mL ≤50.0
初始稠度(180℃、115.0MPa 、86min),Bc ≤30
40~100Bc 的时间,min ≤30
抗压强度(206℃、20.7MPa 、24h),MPa ≥14.0

Swipe horizontally to view the full table.

表 5 加有缓凝型降失水剂的水泥浆和水泥石性能要求
项目指标
失水量,mL ≤100.0
初始稠度(80℃、46.5MPa 、45min),Bc ≤30
40~100Bc 的时间,min ≤30
稠化时间,min ≥120
游离液,% ≤1.4
抗压强度(102℃、20.7MPa 、24h),MPa ≥14.0

Swipe horizontally to view the full table.

表 6 加有抗盐型降失水剂的水泥浆和水泥石性能要求
项目指标
失水量,mL ≤100.0
初始稠度(80℃、46.5MPa 、45min),Bc ≤30
40Bc~100Bc 的时间,min ≤30
游离液,% ≤1.4
抗压强度(102℃、20.7MPa 、24h),MPa ≥14.0

Usage

Dosage and application recommendations are adjusted according to the target fluid system and field conditions.

Samples & small-pack service

In addition, we offer small-packaging and sample services for this product. Bottles, sachets, pails and other package sizes can all be customized to your needs — feel free to contact us.

Product samples

油井用水泥Filtration-Control Additive